2. Specification
Testing Items | Standard | Data |
Appearance | Flat And Smooth | |
Coating Thickness | GB/T6554-2003 | 50~70mm |
Gloss(60°) | GB/T9754-2007 | From 2%~100% to All Gloss |
Impact Resistance | GB/T1732-1993 | 50kg.cm |
Bending Performance | GB/T6742-2007 | 2mm |
Cupping Test | GB/T9753-2007 | 8mm |
Adhesion Force | GB/T9286-1998 | 0 Grade |
Hardness | GB/T6739-2006 | 2H |
Resistant to Salt Test (1000 Hours) | GB/T1771-2007 | No Change For Coating Appearance |
Humidity And Heat Resistance Test (1000 Hours) | GB/T1740-2007 | No Change For Coating Appearance |
Chemical Medium Resistance (240 Hours) 5%H2SO4 5%HCl 5%NaOH 5%NaCl | GB/T1763-1979 |
No Change For Coating Appearance No Change For Coating Appearance No Change For Coating Appearance No Change For Coating Appearance |
Heat Resistance | GB/T1735-2009 | It Can Reach Between 220℃/20minutes And 240℃/40minutes According To Color And Different Requirement |
Artificial Accelerated Aging Test (1000 Hours) (Outdoor) | GB/T1865-2009 | No Change For Coating Appearance |
Test Item | Test Method | Test Result |
Film Thickness | ISO2360 | 60-80um |
Pencil Hardness | ASTMD 3363 | HB-H |
Bending | ISO1519 | ≤10mm |
Grid Test 1mm | ISO2409 | 0 Class |
Impulse Test | ASTMD2794 | Pass |
Cupping Test | ISO1520 | ≥8mm |
Heat Resistance 1000 hours | ISO6270-1 | Popping<1mm |
Salt Spray 1000 hours | ISO9227 | Corrosion Spreading<1mm |